Why formulators use ground rubber
ASTM D5603 sums it up: recycled vulcanizate rubber lets a compounder "add a certain percentage of rubber filler back into its parent or similar compounds or to use the material as substitute or stand alone compound," and "its use may lower compound costs or improve performance characteristics, or both."
The USTMA's 2021 scrap tire report counts this "fine ground rubber" segment, used in new tires, coatings, sealants and exports, at about 79 thousand tons of scrap tires in 2021.
Applications
Hot-pour crack sealants
Rubberized crack sealants blend fine ground rubber into hot asphalt. Finer grinds disperse faster: FHWA's 2020 report notes reaction time in hot binder is a direct function of the rubber's relative surface area, which is why fine GTR such as 80 mesh is used in some binders.

Rubberized coatings and membranes
Foundation and roof coatings, waterproofing membranes and anti-slip coatings use fine rubber for body, flexibility and texture.
Adhesives, mastics and compounds
Fine powders act as functional fillers. Test in your system; finer particles need more polymer or binder to wet out.
Choosing a grind
| Grade | Top size | Best for |
|---|---|---|
| 30-minus | 600 µm | Textured coatings, mastics, high-volume fills. In stock. |
| 40 mesh | ~425 µm (≤10% retained) | Crack sealants, smoother coatings |
| 80 mesh | ~180 µm (≤10% retained) | Fine dispersion, sprayable coatings, compounding |
Worked example
A crack sealant producer's monthly volume
A producer makes 400,000 lb of hot-pour sealant a month. Suppose their formula contains 12% ground rubber by weight:
- 400,000 × 12% = 48,000 lb of 40 mesh a month
- That's about one truckload a month, ~24 supersacks
- Seasonal peak (spring/summer) at 1.5× = 72,000 lb, about 2 loads
Your formula sets the rubber percentage. We set a production schedule so the peak doesn't catch you short.
Send your sealant or coating spec. Send grade, volume, delivery city/ZIP and your target price.
Request a QuoteWhat to put in a fine-grind spec
- Particle size distribution by ASTM D5644 (90 µm and coarser) or a finer method for powders
- Maximum oversize, the particle that clogs your spray tip or shows on the surface
- Residual steel and fiber. Fiber is the enemy of smooth sealants
- Moisture. Water foams hot asphalt and reacts with isocyanates
- Parting agent allowance, if any. Some asphalt-rubber specs, such as ADOT's, have allowed up to 4% calcium carbonate to prevent caking
Frequently asked questions
What mesh rubber is used in crack sealants?
Fine grinds such as 30-minus, 40 and 80 mesh are common. Your formula and equipment decide.
Can you supply rubber powder finer than 80 mesh?
Finer grades are discussed per order. Send your target PSD.
Do you supply trial quantities?
Yes. A lab sample or single supersack for a plant trial.
Will your powder cake in storage?
Fine powders can bridge. Store dry and ask about parting agents if your spec allows.
Sources: ASTM D5603-23 (astm.org), ASTM D5644-23; USTMA 2021 US Scrap Tire Management Summary; FHWA-HIF-20-043 (2020); ADOT §1009 as reproduced in a 2012 specification summary.